Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 850 - 1000 MPa | 123000 - 145000 psi | |
Schmolz + Bickenbach UGICHROM 4028 Martensitic Chrome Plated Bar Description: Ugichrom combines the high efficiency of micro-fissuring chromium plating with the technology of Ugitech’s most advanced gradesAdvantages: Zero defects guarantee; Low friction coef.. |
|||
Tensile Strength at Break | 800 - 1000 MPa | 116000 - 145000 psi | Longitudinal |
Goodfellow Polyaramid/Vinylester Composite Tube or Rod Information provided by Goodfellow. |
|||
Tensile Strength at Break | 650 - 1000 MPa | 94300 - 145000 psi | |
Goodfellow Aluchrom O® Resistance Alloy Resistance heating alloy with excellent resistance to oxidation at elevated temperatures. Used in many varied applications - from small household appliances to large industrial furnaces.Information .. |