Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 9.38 MPa @Temperature 23.0 °C |
1360 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ HC MT224 Thermoplastic Elastomer (TPE) Versaflex™ HC MT224 is an exceptionally clear, high performance TPE developed for medical tubing for healthcare. Versaflex™ HC MT224 has been specially formulated without the use of any plasticize.. |
|||
Tensile Strength at Break | 9.38 MPa | 1360 psi | 510 mm/min; ASTM D412A |
PolyOne Synprene® RT-3790 Styrene Butadiene Block Copolymer (SBC) with Mineral Filler
(discontinued **) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |
|||
Tensile Strength at Break | 9.38 MPa | 1360 psi | ASTM D638 |
LyondellBasell Microthene® G MU76000 Ethylene Vinyl Acetate Copolymer General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Tensile Strength at Break | 9.38 MPa | 1360 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 111-80 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Tensile Strength at Break | 9.38 MPa | 1360 psi | Air at 302°F, 168 hr; ASTM D573 |
ExxonMobil Santoprene® 123-50 Thermoplastic Elastomer
(discontinued **) A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran.. |
|||
Tensile Strength at Break | 9.38 MPa | 1360 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 211-80 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Tensile Strength at Break | 9.38 MPa | 1360 psi | AVG; ASTM D412 Method A |
Seals Eastern 5861 Fluoro-silicone Fluoro-silicone meeting MIL-R-25988BInformation provided by Seals Eastern, Inc. |