Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 8.62 MPa | 1250 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B65B1 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 8.62 MPa | 1250 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible D8000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 8.62 MPa | 1250 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R125AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 8.62 - 10.3 MPa | 1250 - 1500 psi | |
ITW Plexus Plexusâ„¢ MA420FS Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, very fast curing.Information provided by Illinois Tool Works. |
|||
Tensile Strength at Break | 8.62 MPa | 1250 psi | AVG; ASTM D412 Method A |
Seals Eastern 7284 Butyl and Halobutyl Rubber Chlorobutyl; High damping; Non-conductiveInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength at Break | 8.62 MPa | 1250 psi | ASTM D412 |
Teknor Apex Monprene® MP 1166B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.62 MPa | 1250 psi | ASTM D412 |
Teknor Apex Monprene® MP 1225 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.62 MPa | 1250 psi | ASTM D412 |
Teknor Apex Monprene® MP-1504L1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.62 MPa | 1250 psi | ASTM D412 |
Teknor Apex Monprene® MP-1579C Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.62 MPa | 1250 psi | ASTM D412 |
Teknor Apex Monprene® MP-1823 AS Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.62 MPa | 1250 psi | ASTM D412 |
Teknor Apex Monprene® MP-2264R Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.62 MPa | 1250 psi | ASTM D412 |
Teknor Apex Monprene® MP-1393B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.62 MPa | 1250 psi | ASTM D412 |
Teknor Apex Monprene® MP-2602G Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.62 MPa | 1250 psi | ASTM D412 |
Teknor Apex Telcar® OBC 4560A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 8.62 MPa | 1250 psi | ASTM D412 |
Teknor Apex Telcar® OBC 4670A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 8.62 MPa | 1250 psi | ASTM D412 |
Teknor Apex Telcar® TL-1420C Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Grommets; Industrial Soft; Sporting Goods; Toys; Weatherstripping Forms: Pellets Processing Method: Extrusion; Injection Molding Injecti.. |
|||
Tensile Strength at Break | 8.62 MPa | 1250 psi | ASTM D412 |
Teknor Apex Telcar® TL-89-P834-B Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 8.62 MPa | 1250 psi | ASTM D412 |
Teknor Apex Telcar® TL-2580A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | >= 8.62 MPa | >= 1250 psi | |
3M Scotchcal™ ElectroCut™ 406 Graphic Film Product Description:3.25 mil cast film in 6 glossy, opaque, fluorescent colorExtremely conspicuous in daylight and activated by exposure to near ultraviolet light (but not black light)Offers high at.. |
|||
Tensile Strength at Break | >= 8.62 MPa | >= 1250 psi | |
3M Scotchcal™ ElectroCut™ 407 Graphic Film Product Description:3.25 mil cast film in 6 glossy, opaque, fluorescent colorExtremely conspicuous in daylight and activated by exposure to near ultraviolet light (but not black light)Offers high at.. |
|||
Tensile Strength at Break | >= 8.62 MPa | >= 1250 psi | |
3M Scotchcal™ ElectroCut™ 413 Graphic Film Product Description:3.25 mil cast film in 6 glossy, opaque, fluorescent colorExtremely conspicuous in daylight and activated by exposure to near ultraviolet light (but not black light)Offers high at.. |
|||
Tensile Strength at Break | >= 8.62 MPa | >= 1250 psi | |
3M Scotchcal™ ElectroCut™ 414 Graphic Film Product Description:3.25 mil cast film in 6 glossy, opaque, fluorescent colorExtremely conspicuous in daylight and activated by exposure to near ultraviolet light (but not black light)Offers high at.. |
|||
Tensile Strength at Break | >= 8.62 MPa | >= 1250 psi | |
3M Scotchcal™ ElectroCut™ 404 Graphic Film Product Description:3.25 mil cast film in 6 glossy, opaque, fluorescent colorExtremely conspicuous in daylight and activated by exposure to near ultraviolet light (but not black light)Offers high at.. |
|||
Tensile Strength at Break | >= 8.62 MPa | >= 1250 psi | |
3M Scotchcal™ ElectroCut™ 405 Graphic Film Product Description:3.25 mil cast film in 6 glossy, opaque, fluorescent colorExtremely conspicuous in daylight and activated by exposure to near ultraviolet light (but not black light)Offers high at.. |