Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 74.5 MPa | 10800 psi | 2 in/min; ASTM D638 |
RheTech Products F49-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Fan shroudsSupport ductsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 74.5 MPa @Thickness 3.20 mm |
10800 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical Lupox® HI2100M PBT+GF10% Description: Injection Molding, PBT+GF10%, High ImpactApplication: IT/OA, E&E (Bobbin, Switch)CAS No. 65997-17-3, 155123-66-3 and 30965-26-5Information provided by LG Chemical |
|||
Tensile Strength at Break | 74.5 MPa | 10800 psi | ASTM D638 |
Techmer ES Plaslube® NY-1/SI/2 WT PA66 |