Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 66.2 MPa | 9600 psi | 2 in/min; ASTM D638 |
RheTech Products GC20P100-00 15% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 66.2 MPa | 9600 psi | ASTM D638 |
Polymer Resources PC-BR1 Polycarbonate, Branched for Extrusion and Blow Molding Polycarbonate, Branched for Extrusion and Blow MoldingFeatures: • Ultra High Impact Resistance • Ultra High ViscosityProcess: Extrusion/Blow MoldingNotes: All physical, mechanical and thermal te.. |
|||
Tensile Strength at Break | 66.2 MPa | 9600 psi | ASTM D638 |
Polymer Resources PC-BR1-UV Polycarbonate, Branched for Extrusion and Blow Molding, UV-stabilized Polycarbonate, Branched for Extrusion and Blow Molding, UV-stabilizedFeatures: • Ultra High Impact Resistance • Ultra High ViscosityProcess: Extrusion/Blow MoldingNotes: All physical, mechanical.. |
|||
Tensile Strength at Break | 66.2 MPa | 9600 psi | ASTM D638 |
Polymer Resources PC-BR1-[color]-5 Polycarbonate, Branched, Food Contact Polycarbonate, Branched for Extrusion and Blow MoldingFeatures: • Ultra High Impact Resistance • Ultra High Viscosity • Food Contact AcceptableProcess: Extrusion/Blow MoldingNotes: All physica.. |
|||
Tensile Strength at Break | 66.2 MPa | 9600 psi | ASTM D638 |
M. Holland Company PC522UR Polycarbonate High flowHigh impact resistanceGood mold releaseGood UV resistanceApplications: AppliancesProtective coveringsDecorative displaysHousings |
|||
Tensile Strength at Break | 66.2 MPa | 9600 psi | ASTM D638 |
Plastics Group Polifil® GFPC-10 10% Glass-Reinforced Polycarbonate Polifil® GFPC series compounds offer a combination of improved dimensional stability and decreased flammability. The excellent balance of physical properties make the Polifil® glass-filled polycar.. |
|||
Tensile Strength at Break | 66.2 MPa | 9600 psi | 2 in/min; ASTM D638 |
RheTech Products GC20P100-00UV 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Natural Injection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 66.2 MPa | 9600 psi | 2 in/min; ASTM D638 |
RheTech Products GC20P105-08FA 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, FDA Compliant, Black Applications: Water system housingFDA approved partsInjection molding conditions reported in table.Information provided by RheTech Products. |