Mechanical Properties Metric English Comments
Tensile Strength at Break 6.55 MPa
950 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible R5145B Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength at Break 6.55 MPa
950 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible R5145A Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength at Break 6.55 MPa
950 psi
510 mm/min; ASTM D412A
PolyOne Synprene® RT-3880M Styrene Butadiene Block Copolymer (SBC)  (discontinued **)
Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom..
Tensile Strength at Break 6.55 MPa
950 psi
0.010" Thick
GrafTech GRAFOIL® GRAFKOTE® Laminates, Non-Metal Reinforced
GRAFOIL® GRAFKOTE® laminates are made with GRAFOIL® Grade GTB flexible graphite thermally bonded to a 0.0005" thick polymer facing on one ("Single-Sided") or both ("Double-Sided") sides. Th..
Tensile Strength at Break 6.55 MPa
950 psi
DBPH Cure
Shin-Etsu Silicones SV-14000U Silicone Rubber
SV14000U is one of a series of easy processing, no post cure silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendering. Product Feat..
Tensile Strength at Break 6.55 MPa
950 psi
ASTM D412
Teknor Apex Monprene® MP-1881E Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 6.55 MPa
950 psi
ASTM D412
Teknor Apex Monprene® MP-2287C Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 6.55 MPa
950 psi
ASTM D412
Teknor Apex Monprene® MP-2359A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 6.55 MPa
950 psi
ASTM D412
Teknor Apex Monprene® MP-2664A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 6.55 MPa
950 psi
ASTM D412
Teknor Apex Monprene® MP-2664B Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 6.55 MPa
950 psi
ASTM D412
Teknor Apex Telcar® TL-1420A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Tensile Strength at Break 6.55 MPa
950 psi
ASTM D412
Teknor Apex Telcar® TL-1488G Thermoplastic Elastomer
Uses: Flexible Grips; General Purpose; Handles; Household Goods; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast ..
Tensile Strength at Break 6.55 MPa
950 psi
ASTM D412
Teknor Apex Telcar® TL-2318G Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Strength at Break 6.55 MPa
950 psi
ASTM D412
Teknor Apex Telcar® TL-2535A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Strength at Break 6.55 MPa
950 psi
ASTM D412
Teknor Apex Telcar® TL-2550F Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Strength at Break 6.55 MPa
950 psi
ASTM D412
Teknor Apex Telcar® TL-2565A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Strength at Break 6.55 MPa
950 psi
ASTM D412
Teknor Apex Uniprene® UN-7200-73 Thermoplastic Vulcanizate
Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Automotive Specifications: Chrysler MS-AK91; FORD WSS-M2D510-A7; ..
Tensile Strength at Break 6.55 MPa
950 psi
ASTM D412
Teknor Apex Telcar® TL-2470A Thermoplastic Elastomer
Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat..
Tensile Strength at Break 6.55 MPa
950 psi
AFERA 4004
3M Scotch® 8347 Carry Handle Tape
3M™ Carry Handle Tape 8347 is a high-performance tape featuring a durable 3M™ Scotchpro™ Film backing that is longitudinal direction and an aggressive rubber resin adhesive especially suited for ..
Tensile Strength at Break 6.55 MPa
950 psi
ASTM D412
Teknor Apex Monprene® MP-2676B Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 6.55 MPa
950 psi
TM R050-36
Resinlab® SEC1222 Silver Filled Epoxy Adhesive
Resinlab™ SEC1222 is a silver filled, two component, room temperature curing epoxy adhesive. It is designed to cure completely at room temperature. SEC1222 provides excellent electrical conductivit..
Copyright © lookpolymers.com All Rights Reserved