Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 6.27 MPa | 910 psi | Oven cured 4 hours at 480°F |
Malvern Minerals Sliastic 437 with 50% Novacite® L-207A Quartz Filler Press Vulcanized 5 minutes at 260° F. Product data demonstrates the effect of the Novacite® filler.Information provided by Malvern Minerals Company. |
|||
Tensile Strength at Break | 6.27 MPa | 910 psi | ASTM D412 |
Teknor Apex Telcar® OBC 4530A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 6.27 MPa | 910 psi | ASTM D412 |
Teknor Apex Telcar® OBC 4545A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 6.27 MPa | 910 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 251-70W232 Thermoplastic Elastomer A soft, colorable, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance and contains non-ether brominated flame retard.. |
|||
Tensile Strength at Break | 6.27 MPa | 909 psi | 510 mm/min; ASTM D412A |
PolyOne Elastamax™ XL-0153-24 Styrene Butadiene Block Copolymer (SBC)
(discontinued **) A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco.. |