Tensile Strength at Break 6.20 MPa

@Time 7200 sec
899 psi

@Time 2.00 hour
Die C; ASTM D414
STAR Thermoplastic Alloys & Rubbers StarXTRUDE XTR-85-1000 TPE
Product Description: StarXTRUDE XTR-85-1000 is an easy processing TPE designed for extrusion. Features:Soft TouchRubbery FeelMatte finishExcellent chemical and oil resistanceAdherence to PC, ABS & P..
Tensile Strength at Break 6.20 MPa
899 psi
Die C; Cross direction; ASTM D412
Teknor Apex Sarlink® 3160 Thermoplastic Elastomer
A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3160 can be processed by injection molding or extrusion for ap..
Tensile Strength at Break 6.20 MPa
899 psi
Die C; Cross direction; ASTM D412
Teknor Apex Sarlink® 3460 Thermoplastic Elastomer
A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject..
Tensile Strength at Break 6.20 MPa
899 psi
ASTM D638 - ISO 527-2
DuPont Elvaloy® HP4051 Ethylene/N-Butyl Acrylate/Carbon Monoxide Copolymer
Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont.
Tensile Strength at Break 6.20 MPa
899 psi
500mm/min; ASTM D638 Type IV Specimen
Westlake EC812AA Low Density Polyethylene
WESTLAKE low-density polyethylene EC812 is a natural low-density material with a 200 melt index. Its high melt index exhibits excellent wettability. This makes it ideal as a backing to carpet to bin..
Tensile Strength at Break 6.20 MPa
899 psi
Across Flow; ASTM D412 and ISO 37
ExxonMobil Santoprene® 121-70M350 Thermoplastic Vulcanizate - UV Resistant
Product Description: A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for gap filler applications requiring scratch..
Tensile Strength at Break 6.20 MPa
899 psi
Across Flow; ASTM D412 and ISO 37
ExxonMobil Santoprene® 691-65W175 Thermoplastic Vulcanizate
Product Description: A soft, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for thin wall, architectural glazing and sealing applic..
Tensile Strength at Break 6.20 MPa
899 psi
ISO 527-1
Barlog Plastics KEBAFLEX SG 60 A.01 black TPE-S, Shore A60, black
TPE-SInformation provided by BARLOG plastics GmbH.
Tensile Strength at Break 6.20 MPa
899 psi
Die C; Cross direction; ASTM D412
Teknor Apex Sarlink® 3460N Thermoplastic Elastomer
A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext..
Copyright © lookpolymers.com All Rights Reserved