Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 5.00 MPa | 725 psi | ASTM D412 |
Multibase TPSiV™ 3040-55A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Tensile Strength at Break | 5.00 MPa | 725 psi | ISO 37 |
PolyOne OnFlex™ S EH 70A-3S7004 Thermoplastic Elastomer (TPE) OnFlex™-S EH thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver a great cost/performance ratio in addition to t.. |
|||
Tensile Strength at Break | 5.00 MPa | 725 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL WCP700 PPE-TPE Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness. |
|||
Tensile Strength at Break | 5.00 MPa | 725 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL WCP700 PPE-TPE (Asia Pacific) Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness. |
|||
Tensile Strength at Break | 5.00 MPa | 725 psi | ASTM D412 |
Teknor Apex Monprene® MP-1959G Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 5.00 MPa | 725 psi | ASTM D412 |
Teknor Apex Telcar® TL-2530F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 5.00 MPa | 725 psi | ISO 37 |
ELASTO UK Dryflex® 3006-101 TPE, Modified Injection Molding Grade for Auto Interior Parts The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 3006-101 is specifically designe.. |
|||
Tensile Strength at Break | 5.00 MPa | 725 psi | ASTM D638 |
ELASTO UK Dryflex® 500400S SEBS Based Material, Unfilled Qualities, 40A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tensile Strength at Break | 5.00 MPa | 725 psi | ASTM D638 |
ELASTO UK Dryflex® 502400S SEBS Based Material, Unfilled Qualities, 40A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tensile Strength at Break | 5.00 MPa | 725 psi | ASTM D638 |
ELASTO UK Dryflex® 660400S SEBS Based Material, Semi-Filled Qualities, 40A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Tensile Strength at Break | 5.00 MPa | 725 psi | ISO R 527 |
Fainplast Compounds GS 38/T Flexible PVC, Injection Molding for Transparent Technical Items Dolls |
|||
Tensile Strength at Break | 5.00 MPa | 725 psi | ISO R 527 |
Fainplast Compounds GS 39/T Flexible PVC, Injection Molding for Footwear Sandals |
|||
Tensile Strength at Break | 5.00 MPa | 725 psi | ASTM D638 |
ELASTO UK Dryflex® 600400S SEBS Based Material, Filled Qualities, 40A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tensile Strength at Break | 5.00 MPa | 725 psi | ASTM D638 |
Azdel SuperLite® SL552000-100 PP Resin Matrix / 55% Glass Fiber (12 mm Molded Thickness) AZDEL SuperLite® SL552000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Strength at Break | 5.00 MPa | 725 psi | ASTM D638 |
Arkema Group EVATANE® 42-60 Copolymer Ethylene - Vinyl Acetate EVATANE 42-60 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE 42-60 is stabilized with antioxidants and contains slip and antibloc.. |
|||
Tensile Strength at Break | 5.00 MPa | 725 psi | |
Beijing Evergrow Resources GFF-5 Glass Fiber Felt Introduction:By applying high-count fiberglass, GFNF series has the excellent properties such as heat-isolation, fire-resistance, anti-corrosion and heat-preservation. It's the most characteristic a.. |
|||
Tensile Strength at Break | 5.00 MPa | 725 psi | ISO 527 |
Breplast Bretene SP Polypropylene / Polyethylene Composite Recovered polypropylene and polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Tensile Strength at Break | 5.00 MPa | 725 psi | |
LATI Latimass 53-04 D008 PP Homopolymer, Impact Modified Specific density compound based on Polypropylene homopolymer (PPh), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation.. |
|||
Tensile Strength at Break | 5.00 MPa | 725 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon MDM40 PP LNP* Stat-Kon* MDM40 is a compound based on Polypropylene resin containing Mica and Carbon. Characteristics are Statically Conductive.This data was supplied by SABIC-IP for the Americas region. |