Mechanical Properties Metric English Comments
Tensile Strength at Break 43.1 MPa
6250 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® GC-1017 PC/ABS, FR
Information provided by Samsung Cheil Industries.
Tensile Strength at Break 43.1 MPa
6250 psi
50 mm/min; ASTM D638
Supreme Petrochem SC 208 General Purpose Polystyrene
CharacteristicsHigh flow grade Easy processing Good clarity & shineProcessing Extrusion MoldingApplications Hand molding applications of novelty items, toys etc. Carrier for master batches, as a ..
Tensile Strength at Break 43.1 MPa
6250 psi
50 mm/min; ASTM D638
Supreme Petrochem SP 263 Toughened Polystyrene
CharacteristicsGood flexibility Easy flow Good stiffnessProcessing Injection moldingApplications Transparent hangers Material Status: Commercial : ActiveAgency Ratings: FDA 21 CFR 177.1640Informatio..
Tensile Strength at Break 43.1 MPa
6250 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® GC-1017 PC/ABS, FR
Information provided by Samsung Cheil Industries.
Tensile Strength at Break 43.1 MPa
6250 psi
ASTM D295