Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 4.90 MPa | 711 psi | ISO 37 |
PolyOne OnFlex™ S KG 80A-3E2020 Thermoplastic Elastomer (TPE) OnFlex™-S KG thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p.. |
|||
Tensile Strength at Break | 4.90 MPa | 710 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 281-55MED Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad.. |
|||
Tensile Strength at Break | 4.90 MPa | 711 psi | ASTM-F152 |
GrafTech eGRAF® HITHERM™ HT-705 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Tensile Strength at Break | 4.90 MPa | 711 psi | ASTM-F152 |
GrafTech eGRAF® HITHERM™ HT-710 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Tensile Strength at Break | 4.90 MPa | 711 psi | |
Momentive Performance Materials TSE3261-G Heat Resistant Silicone Adhesive TSE3261-G is a one-component heat curable silicone adhesive designed for high temperature applications. TSE3261-G adheres well to a variety of substrates such as metals, plastics, ceramics and glas.. |
|||
Tensile Strength at Break | 4.90 MPa | 710 psi | DBPH Cure |
Shin-Etsu Silicones KE-3611U Electrically Conductive Silicone Elastomer ShinEtsu KE3611 U is a black semi conductive silicone compound. It has been designed as a 60 Durometer material with typical volume resistivity values of 5 W cm.Product Features: Suitable for both m.. |
|||
Tensile Strength at Break | 4.90 MPa | 711 psi | ISO 527 |
A. Schulman INVISION™ VX-5070UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5070UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tensile Strength at Break | 4.90 MPa | 711 psi | ISO 527 |
A. Schulman INVISION™ VX-5070UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5070UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tensile Strength at Break | 4.90 MPa | 711 psi | ISO 527 |
A. Schulman INVISION™ VX-5070UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5070UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tensile Strength at Break | 4.90 MPa | 711 psi | ISO 527 |
A. Schulman INVISION™ VX-5170UE Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5170UE is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy processability, soft touch, low gloss, and exc.. |
|||
Tensile Strength at Break | 4.90 MPa | 711 psi | ISO 527 |
A. Schulman INVISION™ VX-5070UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5070UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tensile Strength at Break | 4.90 MPa | 711 psi | ISO 527 |
A. Schulman INVISION™ VX-5170UE Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5170UE is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy processability, soft touch, low gloss, and exc.. |
|||
Tensile Strength at Break | 4.90 MPa | 711 psi | ISO 527 |
A. Schulman INVISION™ VX-5070UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5070UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tensile Strength at Break | 4.90 MPa | 711 psi | ISO 527 |
A. Schulman INVISION™ VX-5170UE Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5170UE is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy processability, soft touch, low gloss, and exc.. |
|||
Tensile Strength at Break | 4.90 MPa | 711 psi | ISO 527 |
A. Schulman INVISION™ VX-5070UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5070UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tensile Strength at Break | 4.90 MPa | 711 psi | ISO 527 |
A. Schulman INVISION™ VX-5170UE Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5170UE is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy processability, soft touch, low gloss, and exc.. |
|||
Tensile Strength at Break | 4.90 MPa | 711 psi | ISO 527 |
A. Schulman INVISION™ VX-5170UE Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5170UE is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy processability, soft touch, low gloss, and exc.. |
|||
Tensile Strength at Break | 4.90 MPa | 711 psi | ISO 37 |
ELASTO UK Dryflex® 8013-101 Flame Retardant TPE for Extrusion, Black Vitaprene® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Vitaprene® compounds permit sophisticated component design and.. |
|||
Tensile Strength at Break | 4.90 MPa | 711 psi | ISO 37 |
ELASTO UK Dryflex® 8013-101 Flame Retardant TPE for Injection Molding, Black Dryflex® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Dryflex® compounds permit sophisticated component design and thu.. |
|||
Tensile Strength at Break | 4.90 MPa | 710 psi | (20 in/min), Molded Properties; ASTM D638 |
ExxonMobil Escorene™ UL 15019CC Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 15019CC is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applications: Hot.. |
|||
Tensile Strength at Break | 4.90 MPa | 711 psi | Across Flow; ASTM D412 and ISO 37 |
ExxonMobil Santoprene® 121-75M200 Thermoplastic Vulcanizate - UV Resistant Product Description: A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated with high flow properties and exc.. |
|||
Tensile Strength at Break | 4.90 MPa | 710 psi | ASTM D412 |
Aearo E-A-R Specialty Composites VersaDamp™ V-2525 TPE VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded.. |
|||
Tensile Strength at Break | 4.90 MPa | 711 psi | ISO 37 |
Alliance Polymers Viprene™ G45A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G45A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Strength at Break | 4.90 MPa | 711 psi | ISO 37 |
Alliance Polymers Viprene™ G45A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G45A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Strength at Break | 4.90 MPa | 711 psi | ISO 527 |
A. Schulman INVISION™ VX-5170UE Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5170UE is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy processability, soft touch, low gloss, and exc.. |