Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 37.2 MPa | 5400 psi | 2 in/min; ASTM D638 |
RheTech Products F22-01 20% Glass Fiber/Mineral Co-Reinforced Polypropylene, Black Applications: Support ductsHousingsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 37.2 MPa | 5400 psi | ASTM D638 |
Resirene Resirene® HF-777 General Purpose Polystyrene Features:Medium FlowEasy ProcessingMechanical StrengthFDA Rating: 21 CFR 177.1640External Lubrication AvailableApplications:InjectionToysCassette CasesCassettesDisposablesInformation provided by US .. |
|||
Tensile Strength at Break | 37.2 MPa | 5400 psi | |
Indium Corp. Indalloy 160-190 Fusible Bismuth Alloy Information Provided by Indium Corporation |
|||
Tensile Strength at Break | 37.2 MPa | 5400 psi | |
Indium Corp. Indalloy 130 Tin-Lead Solder Alloy Inexpensive utility solderInformation Provided by Indium Corporation |
|||
Tensile Strength at Break | 37.2 MPa | 5400 psi | ASTM D638 |
Chase Plastics CP Pryme® A100HI ABS Molding Resin, High Impact Information provided by Chase Plastics. |
|||
Tensile Strength at Break | 37.2 MPa | 5400 psi | 74% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Trichloroethylene for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Tensile Strength at Break | 37.2 MPa | 5400 psi | vs. aluminum; 90 s set time |
Elmer's Products Aron Alpha® 403TB Cyanoacrylate Adhesive (Industrial Krazy Glue™) Extra tough adhesives with highest heat, peeling, impact and thermal shock resistance.High gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Excellent on metal substrates. Fa.. |
|||
Tensile Strength at Break | 37.2 MPa | 5400 psi | ASTM D638 |
Americas Styrenics STYRON® 678D High Heat Crystal Polystyrene Product CharacteristicsHigh heat resistanceExcellent clarityGood moldabilityFood Contact CompliantTypical ApplicationsDisposable cutleryHousewaresCompact disc and DVD jewel boxesDesk organizersInfor.. |
|||
Tensile Strength at Break | 37.2 MPa | 5400 psi | ASTM D638 |
ExxonMobil Paxon™ BA7718 Sheet Extrusion and Blow Molding Resin
(discontinued **) BA7718 is a 25% brown mica-filled, medium molecular weight, high density polyethylene. This material has been specifically developed as a cost effective resin for applications which require outstan.. |