Mechanical Properties Metric English Comments
Tensile Strength at Break 3600 MPa
522000 psi
ASTM D3379-101
SGL Carbon Group SIGRAFIL C® C25 M350 UNS Milled Carbon Fiber, Unsized Carbon Fiber
Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG..
Tensile Strength at Break 3600 MPa
522000 psi
ASTM D3379-103
SGL Carbon Group SIGRAFIL C® C25 P250 EPY Pelletized Carbon Fiber, Epoxy Sizing
Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG..
Tensile Strength at Break 3600 MPa
522000 psi
ASTM D3379-104
SGL Carbon Group SIGRAFIL C® C25 P350 GLY Pelletized Carbon Fiber, Glycerine Sizing
Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG..
Tensile Strength at Break 3600 MPa
522000 psi
ASTM D3379-102
SGL Carbon Group SIGRAFIL C® C25 P350 PUT Pelletized Carbon Fiber, Polyurethane Sizing
Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG..
Tensile Strength at Break 3600 MPa
522000 psi
ASTM D3379-83
SGL Carbon Group SIGRAFIL C® C25 S001 EPY Staple Carbon Fiber, Epoxy Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Tensile Strength at Break 3600 MPa
522000 psi
ASTM D3379-81
SGL Carbon Group SIGRAFIL C® C25 S003 APS Staple Carbon Fiber, Aromatic Polymer Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Tensile Strength at Break 3600 MPa
522000 psi
ASTM D3379-84
SGL Carbon Group SIGRAFIL C® C25 S003 EPY Staple Carbon Fiber, Epoxy Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Tensile Strength at Break 3600 MPa
522000 psi
ASTM D3379-88
SGL Carbon Group SIGRAFIL C® C25 S003 GLY Staple Carbon Fiber, Glycerine Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Tensile Strength at Break 3600 MPa
522000 psi
ASTM D3379-79
SGL Carbon Group SIGRAFIL C® C25 S003 PUT Staple Carbon Fiber, Polyurethane Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Tensile Strength at Break 3600 MPa
522000 psi
ASTM D3379-82
SGL Carbon Group SIGRAFIL C® C25 S006 APS Staple Carbon Fiber, Aromatic Polymer Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Tensile Strength at Break 3600 MPa
522000 psi
ASTM D3379-85
SGL Carbon Group SIGRAFIL C® C25 S006 EPY Staple Carbon Fiber, Epoxy Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Tensile Strength at Break 3600 MPa
522000 psi
ASTM D3379-89
SGL Carbon Group SIGRAFIL C® C25 S006 GLY Staple Carbon Fiber, Glycerine Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Tensile Strength at Break 3600 MPa
522000 psi
ASTM D3379-80
SGL Carbon Group SIGRAFIL C® C25 S006 PUT Staple Carbon Fiber, Polyurethane Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Tensile Strength at Break 3600 MPa
522000 psi
ASTM D3379-86
SGL Carbon Group SIGRAFIL C® C25 S009 EPY Staple Carbon Fiber, Epoxy Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Tensile Strength at Break 3600 MPa
522000 psi
ASTM D3379-90
SGL Carbon Group SIGRAFIL C® C25 S009 GLY Staple Carbon Fiber, Glycerine Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Tensile Strength at Break 3600 MPa
522000 psi
ASTM D3379-87
SGL Carbon Group SIGRAFIL C® C25 S012 EPY Staple Carbon Fiber, Epoxy Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Tensile Strength at Break 3600 MPa
522000 psi
ASTM D3379-91
SGL Carbon Group SIGRAFIL C® C25 S012 GLY Staple Carbon Fiber, Glycerine Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Tensile Strength at Break 3600 MPa
522000 psi
ASTM D3379-99
SGL Carbon Group SIGRAFIL C® C25 M100 UNS Milled Carbon Fiber, Unsized Carbon Fiber
Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG..
Tensile Strength at Break 3600 MPa
522000 psi
ASTM D3379-100
SGL Carbon Group SIGRAFIL C® C25 M250 UNS Milled Carbon Fiber, Unsized Carbon Fiber
Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG..
Copyright © lookpolymers.com All Rights Reserved