Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 34.1 MPa | 4940 psi | ASTM D882 |
Westlake Plastics ECTFE Film Made from HALAR® Ethylene-chlorotrifluoroethylene Resin Excellent purity. Excellent chemical resistance. Low permeability. Excellent abrasion resistance. Excellent temperature resistance.Halar® is a trade name of Solvay Solexis, Inc. Information p.. |
|||
Tensile Strength at Break | 34.1 MPa | 4950 psi | 68% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Methanol for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |