Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 2.21 MPa | 320 psi | Air at 212°F, 1008 hr; ASTM D573 |
ExxonMobil Santoprene® 121-65M300 Thermoplastic Elastomer
(discontinued **) A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and good.. |
|||
Tensile Strength at Break | 2.21 MPa | 320 psi | ASTM D412 |
Teknor Apex Telcar® TL-88-N873K BLK 111 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 2.21 MPa | 320 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8211-25 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Tensile Strength at Break | 2.21 MPa | 321 psi | JRF- 72 hrs @ 60°C, and 72 hrs @ 49°C Air Drying, and 7 days @ 121°C |
3M AC-350 Class A-1 Aerospace Sealant 3M Aerospace Sealant AC-350 Class A are fast-cure, intermediate density two-component, manganese dioxide cure, brushable, polysulfide fuel tank and fuselage sealants. 3M AC-350 Class A Sealants have.. |
|||
Tensile Strength at Break | 2.21 MPa | 321 psi | JRF- 72 hrs @ 60°C, and 72 hrs @ 49°C Air Drying, and 7 days @ 121°C |
3M AC-350 Class A-1/2 Aerospace Sealant 3M Aerospace Sealant AC-350 Class A are fast-cure, intermediate density two-component, manganese dioxide cure, brushable, polysulfide fuel tank and fuselage sealants. 3M AC-350 Class A Sealants have.. |
|||
Tensile Strength at Break | 2.21 MPa | 321 psi | JRF- 72 hrs @ 60°C, and 72 hrs @ 49°C Air Drying, and 7 days @ 121°C |
3M AC-350 Class A-2 Aerospace Sealant 3M Aerospace Sealant AC-350 Class A are fast-cure, intermediate density two-component, manganese dioxide cure, brushable, polysulfide fuel tank and fuselage sealants. 3M AC-350 Class A Sealants have.. |