Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 13.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 13.3 MPa
1930 psi
Across flow; ASTM D412
Advanced Elastomer Systems Santoprene® 8281-90 Thermoplastic Rubber  (discontinued **)
Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other ..
Tensile Strength at Break 13.3 MPa
1930 psi
Shin-Etsu Silicones FE-341U Fluorosilicone Elastomer
ShinEtsu FE341 U is one of a series of high tensile, high tear fluorosilicone compounds. It is designed to process well in molding applications. It can be blended with other members of the series fo..
Tensile Strength at Break 13.3 MPa
1930 psi
ASTM D638
Teknor Apex Flexalloy® 9602-72FR Polyvinyl Chloride, Elastomer
Notes: 105°C Jacket; RoHS Compliant Features: Flame Retardant; High Heat Resistance; Low Temperature Flexibility; Sunlight Resistant (720 hours) Uses Cable Jacketing Wire Types: SEOW; SEW; SJEOW;..
Tensile Strength at Break 13.3 MPa
1930 psi
ASTM D412
Teknor Apex Monprene® MP-2455N Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 13.3 MPa
1930 psi
Post Cure 16 Hours @ 230°C
3M Dyneon™ LTFE 6400Z Low Temperature Fluoroelastomer
3M™ Dyneon™ Low Temperature Fluoroelastomers LTFE 6400Z are technically advanced low temperature, peroxide-cured fluoroelastomers, designated as a FKM type 3 elastomer per ASTM D1418. They are des..
Tensile Strength at Break 13.3 MPa
1930 psi
Post Cure 16 Hours @ 230°C
3M Dyneon™ LTFE 6400ZC Low Temperature Fluoroelastomer
3M™ Dyneon™ Low Temperature Fluoroelastomers LTFE 6400ZC are technically advanced low temperature, peroxide-cured fluoroelastomers, designated as a FKM type 3 elastomer per ASTM D1418. They are de..
Tensile Strength at Break 13.3 MPa
1930 psi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FE 5610 Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FE 5610 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul..