Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 12.5 MPa | 1810 psi | ASTM D638 |
Petroquimica Triunfo Trithene® CX 7020 LDPE - Cast Film The Trithene® CX 7020 resin is a low-density polyethylene (LDPE) with medium molecular weight, excellent processability, and low gel content. Those features allow a production of thin and highly un.. |
|||
Tensile Strength at Break | 12.5 MPa | 1810 psi | ASTM D638 |
Petroquimica Triunfo Trithene® SX 7010 LDPE - Blow Molding The Trithene® SX 7010 resin is a medium molecular weight, low-density polyethylene (LDPE) which allows the production of flasks with an adequate combination of mechanical and impact strength, flexi.. |
|||
Tensile Strength at Break | 12.5 MPa | 1810 psi | ASTM D638 |
Petroquimica Triunfo Trithene® TS 7010 LDPE - Medium Duty Packaging The Trithene TS 7010 resin is a low-density polyethylene (LDPE) with a high molecular weight, excellent processability, and good mechanical properties. The incorporated additives package warrants th.. |
|||
Tensile Strength at Break | 12.5 MPa | 1810 psi | ASTM D638 |
Petroquimica Triunfo Trithene® TS 7028 LDPE - Automatic Packaging The Trithene TS 7028 resin is a low-density polyethylene (LDPE) with excellent optical and processability properties that allows for the production of films combining appearance, mechanical strength.. |
|||
Tensile Strength at Break | 12.5 MPa | 1810 psi | ASTM D638 |
Petroquimica Triunfo Trithene® TX 7010 LDPE - Medium Duty Film The Trithene® TX 7010 resin is a low-density polyethylene (LDPE) with high molecular weight, excellent processability with very good mechanical properties. Besides these properties, the material is.. |
|||
Tensile Strength at Break | 12.5 MPa | 1810 psi | IEC 60811 |
Solvay Specialty Polymers Cogegum® AFR/765 Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Tensile Strength at Break | 12.5 MPa | 1810 psi | IEC 60811 |
Solvay Specialty Polymers Cogegum® AFR/960 Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Tensile Strength at Break | 12.5 MPa | 1810 psi | IEC 60811 |
Solvay Specialty Polymers Cogegum® GFR/360 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Tensile Strength at Break | 12.5 MPa | 1810 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible FC800 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 12.5 MPa | 1810 psi | ASTM D638 |
Solvay Specialty Polymers Cogegum® AFR/710 Polyolefin Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties witho.. |
|||
Tensile Strength at Break | 12.5 MPa | 1810 psi | ASTM D638 |
Solvay Specialty Polymers Cogegum® GFR/360 Polyolefin Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a poly.. |
|||
Tensile Strength at Break | 12.5 MPa | 1810 psi | ISO R 527 |
Stir SpA POROCELL Z 559 AT (PVC) Application: Matt super foam for injection moldingInformation provided by STIR SpA |
|||
Tensile Strength at Break | 12.5 MPa | 1810 psi | ISO R 527 |
Stir SpA SA 68 R (PVC) Application: Extrusion matt and sheath CEI 20-11 type TM-2Information provided by STIR SpA |
|||
Tensile Strength at Break | 12.5 MPa | 1810 psi | ISO R 527 |
Stir SpA SR 78 REF CZ (PVC) Application: Extrusion pipes and ecological sheath CEI 20-11 type TM 2Information provided by STIR SpA |
|||
Tensile Strength at Break | 12.5 MPa | 1810 psi | ASTM D638 |
Teknor Apex APEX® 91-A1386C-63NT Polyvinyl Chloride, Flexible Notes: RoHS Compliant Uses: Medical/Healthcare Applications Forms: PelletsInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 12.5 MPa | 1810 psi | 25mm/min; ISO 527 |
Borealis LE0563 Polyethylene Compound, Thermoplastic, Semiconductive LE0563 is a thermoplastic semi conductive compound specifically designed for medium- and high voltage cable systems requiring improved grounding. It may be used either as a complete jacket or as a t.. |
|||
Tensile Strength at Break | 12.5 MPa | 1810 psi | ISO 527-2 |
ExxonMobil Exxtral™ BMU130P Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance for automotive exterior applications such as bumper fascia.Availability: Asia Paci.. |
|||
Tensile Strength at Break | 12.5 MPa | 1810 psi | |
Daikin DAI-EL G-558 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 69% Fluorine Content Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Low gasoline permeability and good.. |
|||
Tensile Strength at Break | >= 12.5 MPa | >= 1810 psi | 50 mm/min; ISO 527 |
Fainplast Compounds Ethylplus 615 MD Polyethylene Cable Compound Polyethelene, halogen-free cable compound with superior thermo-mechanical properties, outstanding heat resistance, and high electrical propertiesSolid MDPEInformation provided by Fainplast Compounds.. |
|||
Tensile Strength at Break | 12.5 MPa | 1810 psi | IEC 60811 |
Fainplast Compounds HAX HF 045 Halogen Free PVC General purpose; improved fire performance |
|||
Tensile Strength at Break | 12.5 MPa | 1810 psi | IEC 60811 |
Fainplast Compounds HAX HFX 024-21L Halogen Free PVC This product is a LSFOH silane grafted compound for cable insulation and sheating, cross-linking by heat and moisture by previous addition of a suitable catalyst masterbatch. It is highly recommende.. |
|||
Tensile Strength at Break | 12.5 MPa | 1810 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8281-90MED Thermoplastic Elastomer A hard, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Tensile Strength at Break | 12.5 MPa | 1810 psi | ASTM D3759 |
3M 856 General Purpose Polyester Tape 3M™ General Purpose Polyester Tape 856 is a transparent polyester film tape for edging and reinforcing applications.Information provided by 3M |
|||
Tensile Strength at Break | 12.5 MPa | 1810 psi | ASTM D638 |
Solvay Specialty Polymers Cogegum® AFR/960 Polyolefin Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties withou.. |
|||
Tensile Strength at Break | 12.5 MPa | 1810 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 111-87 Thermoplastic Elastomer
(discontinued **) A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Tensile Strength at Break | 12.5 MPa | 1810 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 211-87 Thermoplastic Elastomer
(discontinued **) A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Tensile Strength at Break | 12.5 MPa | 1810 psi | ISO R 527 |
Fainplast Compounds PM 6510 Flexible PVC, Lead Free Gaskets for frames stabilized Ca-Zn |
|||
Tensile Strength at Break | 12.5 MPa | 1810 psi | IEC 60811 |
Solvay Specialty Polymers Cogegum® AFR/710 Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |