Mechanical Properties Metric English Comments
Tensile Strength at Break 0.517 MPa
75.0 psi
3M 12049 Black 3/8" (9.5 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Tensile Strength at Break 0.517 MPa
75.0 psi
3M 12050 Black 1/2" (12.7 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Tensile Strength at Break 0.517 MPa
75.0 psi
3M 12062 Black 3/32" (2.4 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Tensile Strength at Break 0.517 MPa
75.0 psi
3M 12046 Black 1/16" (1.6 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Tensile Strength at Break 0.517 MPa
75.0 psi
3M 12048 Black 1/8" (3.2 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Tensile Strength at Break 0.517 MPa
75.0 psi
3M 12054 Black 1/4" (6.4 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Tensile Strength at Break 0.517 MPa
75.0 psi
3M 12056 Black 3/16" (4.8 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Tensile Strength at Break >= 0.517 MPa
>= 75.0 psi
ASTM D412
Parker Chomerics CHO-FORM 5531 EMI Shielding Material
One component, moisture cure, form-in-place EMI gasketing material. This electrically conductive formulation contains silver-plated copper particles dispersed in a silicone elastomer. It is designed..