Mechanical Properties Metric English Comments
Izod Impact, Unnotched 2.1356 - 2.1356 J/cm

@Temperature -40.0 - -40.0 °C
4.0009 - 4.0009 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 2.14 J/cm Grade Count:1
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values..
Izod Impact, Unnotched 0.58729 - 2.1356 J/cm

@Temperature -40.0 - -40.0 °C
1.1002 - 4.0009 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 1.14 J/cm Grade Count:8
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Sheet". Each property range of values reported is minimum and max..
Izod Impact, Unnotched 2.1356 - 2.1356 J/cm

@Temperature -18.0 - -18.0 °C
4.0009 - 4.0009 ft-lb/in

@Temperature -0.400 - -0.400 °F
Average value: 2.14 J/cm Grade Count:1
Overview of materials for Polypropylene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri..
Izod Impact, Unnotched 2.02882 - 2.1356 J/cm

@Temperature -18.0 - -18.0 °C
3.80081 - 4.0009 ft-lb/in

@Temperature -0.400 - -0.400 °F
Average value: 2.06 J/cm Grade Count:3
Overview of materials for Polypropylene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of..