Izod Impact, Unnotched 1.07 - 2.14 J/cm
2.00 - 4.00 ft-lb/in
Average value: 1.74 J/cm Grade Count:6
Overview of materials for PPE/PPO + Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "PPE/PPO + Carbon Fiber". Each property range of values reported is minimum and maximum values of appropr..
Izod Impact, Unnotched 0.908 - 2.14 J/cm
1.70 - 4.00 ft-lb/in
Average value: 1.43 J/cm Grade Count:8
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler". Specific grades with glass content between 5% ..
Izod Impact, Unnotched 1.60 - 2.14 J/cm

@Thickness 3.17 mm
3.00 - 4.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® ASA GF15 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: UV StabilizerFeatures: Good UV ResistanceInformation provided by TP Composites..
Izod Impact, Unnotched 1.60 - 2.14 J/cm

@Thickness 3.17 mm
3.00 - 4.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® ASA GF20 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: UV StabilizerFeatures: Good UV ResistanceInformation provided by TP Composites..
Izod Impact, Unnotched 1.07 - 2.14 J/cm
2.00 - 4.00 ft-lb/in
Bulk Molding Compounds BMC 610 Mineral filled, glass-fiber-reinforced polyester compound
BMC 610 molding compound is a mineral filled, glass­ fiber­ reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is set a part form other medium impact..
Izod Impact, Unnotched 1.60 - 2.14 J/cm
3.00 - 4.00 ft-lb/in
Average value: 1.80 J/cm Grade Count:4
Overview of materials for Acrylic, Glass Fiber Reinforced