Izod Impact, Unnotched 6.41 - 10.1 J/cm
12.0 - 19.0 ft-lb/in
Average value: 7.53 J/cm Grade Count:10
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35..
Izod Impact, Unnotched 7.47 - 10.1 J/cm
14.0 - 19.0 ft-lb/in
Average value: 8.68 J/cm Grade Count:4
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45..
Izod Impact, Unnotched 9.10 - 10.1 J/cm
17.0 - 19.0 ft-lb/in
Average value: 9.74 J/cm Grade Count:4
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled". Each property range of values reported i..
Izod Impact, Unnotched 1.57 - 10.1 J/cm
2.94 - 19.0 ft-lb/in
Average value: 7.43 J/cm Grade Count:29
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..
Izod Impact, Unnotched 4.27 - 10.1 J/cm
8.00 - 19.0 ft-lb/in
Average value: 6.89 J/cm Grade Count:10
Overview of materials for Nylon 66, 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc..
Izod Impact, Unnotched 7.47 - 10.1 J/cm
14.0 - 19.0 ft-lb/in
ASTM D4812
Premix Premi-Glas® 1200H-24 Polyester SMC  (discontinued **)
Premi-Glas® 1200H-24 is a 24% fiberglass reinforced, thermoset, Sheet Molding Compound designed for applications where arc resistance and dielectric strength are required and UL 94 HB flame recogni..