Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.38 J/cm @Thickness 3.18 mm |
8.21 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Stat-Kon® OC-1006 Polyphenylene Sulfide, Carbon Fiber Reinforcement
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Izod Impact, Unnotched | 4.38 J/cm | 8.21 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® A-1115 HS Polyphthalamide (PPA) Resin, 15% Glass Reinforced, Dry As Molded
AMODEL A-1115 HS resin is a 15% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, and high tensile strength. Excellent cre.. |
|||
Izod Impact, Unnotched | 4.38 J/cm | 8.21 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Comtuf® 106 Polypropylene, Glass/Mineral Reinforced, Chemically Coupled, Impact Modified, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass/Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has .. |
|||
Izod Impact, Unnotched | 4.38 J/cm | 8.21 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 446 Glass/Mineral Reinforced, PET Alloy Data provided by the manufacturer, ComAlloy International Company.35% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |