Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.27 J/cm @Thickness 3.17 mm |
8.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® PC CF10 TL15 FR BK 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightAdditive: PTFE LubricantFeatures: Lubricated and Flame RetardantAppearance: BlackInformation provided.. |
|||
Izod Impact, Unnotched | 4.27 J/cm @Temperature 23.0 °C |
8.00 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp EC002E PEI LNP THERMOCOMP* EC002E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas.. |
|||
Izod Impact, Unnotched | 4.27 J/cm | 8.00 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP JF003E PES (Asia Pacific) LNP* Thermocomp* JF003E is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
Izod Impact, Unnotched | 4.27 J/cm | 8.00 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM HU2410 PEI (Asia Pacific) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Izod Impact, Unnotched | 4.27 J/cm | 8.00 ft-lb/in | At 73°F; ASTM D256 |
Plastics Group Polifil® C-10 10% Calcium Carbonate-Reinforced Polypropylene Polifil® C series compounds are homopolymer polypropylene resins reinforced with fine particle size calcium carbonate. They combine high impact with stiffness, heat aging, good colorability, resist.. |