Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 3.65 J/cm | 6.84 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 1200-10 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-10 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Izod Impact, Unnotched | 3.65 J/cm | 6.84 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 1200H-10 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200H-10 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:G.. |