Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.99 J/cm | 5.60 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON ZE004 MODIFIED POLYPHENYLENE (Asia Pacific) LNP* Stat-kon* ZE004 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber. |
|||
Izod Impact, Unnotched | 2.99 J/cm @Temperature 23.0 °C |
5.60 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Stat-kon ZE004 MODIFIED POYPHENYLENE LNP* Stat-kon* ZE004 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 2.99 J/cm @Temperature 23.0 °C |
5.60 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Stat-kon ZE004 MODIFIED POYPHENYLENE (Asia Pacific) LNP* Stat-kon* ZE004 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Unnotched | 2.99 J/cm | 5.60 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON ZE004 PPO LNP* STAT-KON* ZE004 is a compound based on PPO resin containing 20% Carbon Fiber. Added feature of this grade includes: Electrically Conductive. |
|||
Izod Impact, Unnotched | 2.99 J/cm | 5.60 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RF002ES PA 66 LNP THERMOCOMP* RF002ES is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Izod Impact, Unnotched | 2.99 J/cm | 5.60 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP WFB54 PBT LNP* THERMOCOMP* WFB54 is a compound based on PBT resin containing 20% Glass Fiber, 25% Glass Bead. |
|||
Izod Impact, Unnotched | 2.99 J/cm | 5.60 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP WFB54 PBT (Asia Pacific) LNP* Thermocomp* WFB54 is a compound based on Polybutylene Terephalate resin containing Glass Bead. |
|||
Izod Impact, Unnotched | 2.99 J/cm | 5.60 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP MC002 PP LNP* THERMOCOMP* MC002 is a compound based on Polypropylene resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Unnotched | 2.99 J/cm | 5.60 ft-lb/in | At 73°F; ASTM D256 |
Plastics Group Polifil® GFABS-10 10% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS) Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.Applications: Fire.. |