Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.08 - 5340 J/cm | 3.90 - 10000 ft-lb/in | Average value: 7.33 J/cm Grade Count:55 |
Overview of materials for Polycarbonate, Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val.. |
|||
Izod Impact, Unnotched | 2.08 J/cm - NB | 3.90 ft-lb/in - NB | Average value: 5.69 J/cm Grade Count:7 |
Overview of materials for Polypropylene, Mineral Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced, Impact Modified". Each property range of values reported is minimum a.. |
|||
Izod Impact, Unnotched | 2.08 - 4.43 J/cm | 3.90 - 8.30 ft-lb/in | Average value: 2.97 J/cm Grade Count:13 |
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is .. |
|||
Izod Impact, Unnotched | 2.08 J/cm @Thickness 3.17 mm |
3.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Fiberfil® PP-62/MI/25 Polypropylene Copolymer, 25% Mica Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Izod Impact, Unnotched | 2.08 J/cm | 3.90 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP KZL16 Acetal Copolymer LNP LUBRICOMP* KZL16 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 2.08 J/cm | 3.90 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON AX00756 ABS LNP STAT-KON* AX00756 is a compound based on ABS resin containing Stainless Steel. Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Unnotched | 2.08 J/cm | 3.90 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RF006LXP PA 66 (Asia Pacific) LNP* Thermocomp* RF006LXP is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Low Extractible. |
|||
Izod Impact, Unnotched | 2.08 J/cm | 3.90 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Comtuf® 101 Polypropylene, Mineral Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.25% Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i.. |
|||
Izod Impact, Unnotched | 2.08 J/cm | 3.90 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Voloy® 688 Nylon 6/6, Glass Fiber/Bead Reinforced, Nylon 6/6 Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.45% Glass Fiber/Bead Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman prod.. |