Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 9.00 J/cm | 16.9 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 1261-28 VE Glass Reinforced Vinyl Ester TMC Description: Premi-Glas® 1261-28 VE is a glass reinforced vinyl ester molding compound designed for automotive under the hood applications. Key features and benefits: Excellent thermal stability an.. |
|||
Izod Impact, Unnotched | 9.00 J/cm | 16.9 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 2200-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Izod Impact, Unnotched | 9.00 J/cm | 16.9 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 2203-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Izod Impact, Unnotched | 9.00 J/cm | 16.9 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 2203-22 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-22 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
Izod Impact, Unnotched | 9.00 J/cm | 16.9 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 2204-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Izod Impact, Unnotched | 9.00 J/cm | 16.9 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 2205-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Izod Impact, Unnotched | 9.00 J/cm | 16.9 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 3140-22 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 3140-22 is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves glass.. |
|||
Izod Impact, Unnotched | 9.00 J/cm | 16.9 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 3200-22 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-22 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Izod Impact, Unnotched | 9.04 J/cm | 16.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP PFL38S PA 6 LNP* LUBRICOMP* PFL38S is a compound based on Nylon 6 resin containing 40% Glass Fiber, 15% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant |
|||
Izod Impact, Unnotched | 9.04 J/cm | 16.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP RX05496 PA 66 LNP* LUBRICOMP* RX05496 is a compound based on Nylon 66 resin containing 30% Mixed Glass, 15% PTFE, Silicone. Added features of this material include: Wear Resistant. |
|||
Izod Impact, Unnotched | 9.04 J/cm | 16.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP RX05496 PA 66 (Asia Pacific) LNP* Lubricomp* RX05496 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 9.00 J/cm | 16.9 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA), 60% Glass Fiber (Dry) Ixef® 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Featur.. |
|||
Izod Impact, Unnotched | 9.01 J/cm | 16.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DF005 PC LNP* Thermocomp* DF005 is a compound based on Polycarbonate containing 25% Glass Fiber. |
|||
Izod Impact, Unnotched | 9.00 J/cm | 16.9 ft-lb/in | ASTM D256A |
Total PPH 3462 Polypropylene, Extrusion Grade Homopolymer extrusion grade for slit film and fibrillated tapesProcess Stability --FINA 3462 is formulated to give excellent process stability in extrusion applications.FDA - FINA 3462 complies with.. |
|||
Izod Impact, Unnotched | 9.00 J/cm | 16.9 ft-lb/in | ISO 180 |
Solvay Specialty Polymers Ixef® 1313/0004 Polyarylamide, 40% Glass Fiber + Elastomer, DAM
(discontinued **)&l Impact modified. The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manu.. |