Polymer Property : Izod Impact, Unnotched = 1.84 ft-lb/in - NB Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.981 J/cm - NB
1.84 ft-lb/in - NB
Average value: 13.3 J/cm Grade Count:26
Overview of materials for Polycarbonate, UV Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a..
Izod Impact, Unnotched 0.981 - 11.2 J/cm
1.84 - 21.0 ft-lb/in
Average value: 7.34 J/cm Grade Count:21
Overview of materials for Polycarbonate, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E..
Izod Impact, Unnotched 0.981 J/cm
1.84 ft-lb/in
ASTM D256
Hyosung Topilene HJ541CP PP
HJ541CP High Isostatic PP Impact CopolymerApplications:Cap of pressure bottleCharacteristics:High stiffnessSlip propertyMedium impactInformation provided by Hyosung Corporation
Izod Impact, Unnotched 0.981 J/cm
1.84 ft-lb/in
ASTM D256
Hyosung Topilene J640 PP
J640 Injection Impact CopolymerApplications:General purposeBattery caseElectric applianceCharacteristics:Medium ImpactFlowabilityInformation provided by Hyosung Corporation
Izod Impact, Unnotched 0.981 J/cm
1.84 ft-lb/in
ASTM D256
Hyosung Topilene J640U PP
J640U Injection Impact CopolymerApplications:General purposeBattery caseElectric applianceCharacteristics:Medium ImpactFlowabilityWeatherabilityInformation provided by Hyosung Corporation
Izod Impact, Unnotched 0.981 J/cm
1.84 ft-lb/in
ASTM D256
Hyosung Topilene J642 PP
J642 Injection Impact CopolymerApplications:Washing M/C partsElectric applianceCharacteristics:Medium impactHigh stiffnessInformation provided by Hyosung Corporation
Izod Impact, Unnotched 0.981 J/cm
1.84 ft-lb/in
ASTM D256
Hyosung Topilene R301 PP
R301 Extrusion Random CopolymerApplications:Extrusion blow moldingThermoforming sheetCharacteristics:TransparencyStiffnessStretchabilityInformation provided by Hyosung Corporation
Izod Impact, Unnotched 0.981 J/cm - NB
1.84 ft-lb/in - NB
Average value: 7.89 J/cm Grade Count:12
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma..
Izod Impact, Unnotched 0.981 J/cm

@Thickness 3.17 mm
1.84 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samyang Trirex® 3025GRU30 Polycarbonate, 30% Glass Reinforced
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, electr..