Polymer Property : Izod Impact, Unnotched = 1.57 ft-lb/in
Polymer Property :
Izod Impact, Unnotched =
1.57 ft-lb/in
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Izod Impact, Unnotched
0.840
J/cm
1.57
ft-lb/in
ASTM D256
North Wood Plastics Polypropylene with 40% Wood Fiber, Molding Grade
Data provided by North Wood Plastics, Inc.