Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP VERTON EV008 PEI LNP* VERTON* EV008 is a compound based on Polyetherimide containing 40% Long Glass Fiber. Added feature of this grade is: Structural. |
|||
Izod Impact, Unnotched | 0.420 - 1.00 J/cm | 0.787 - 1.87 ft-lb/in | Notch Status Unknown |
Goodfellow Nickel Base Magnetic Shielding Alloy - Mu Metal High Nickel magnetically soft alloy used for magnetic shielding, high quality but low noise audio frequency transformers, ground fault interrupter cores, anti-shoplifting devices, tape recorder head.. |
|||
Izod Impact, Unnotched | 0.420 - 1.00 J/cm | 0.787 - 1.87 ft-lb/in | Notch Status Unknown |
Goodfellow Evanohm® Precision Resistance Nickel Alloy Electrical resistance alloy with a very low temperature coefficient of resistivityInformation provided by Goodfellow. |