Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.801 - 8.54 J/cm | 1.50 - 16.0 ft-lb/in | Average value: 5.11 J/cm Grade Count:44 |
Overview of materials for Polycarbonate, Carbon + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + PTFE Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Izod Impact, Unnotched | 2.14 - 8.54 J/cm | 4.00 - 16.0 ft-lb/in | Average value: 4.14 J/cm Grade Count:14 |
Overview of materials for Liquid Crystal Polymer (LCP), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Carbon Fiber Filled". Each property range of values reported is minimum an.. |
|||
Izod Impact, Unnotched | 3.20 - 8.54 J/cm @Temperature -40.0 - -40.0 °C |
5.99 - 16.0 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 5.00 J/cm Grade Count:4 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi.. |
|||
Izod Impact, Unnotched | 3.20 - 8.54 J/cm @Thickness 3.20 - 81.3 mm |
5.99 - 16.0 ft-lb/in @Thickness 0.126 - 3.20 in |
Average value: 5.00 J/cm Grade Count:4 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi.. |
|||
Izod Impact, Unnotched | 3.47 - 8.54 J/cm | 6.50 - 16.0 ft-lb/in | Average value: 5.84 J/cm Grade Count:14 |
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma.. |
|||
Izod Impact, Unnotched | 3.74 - 8.54 J/cm | 7.00 - 16.0 ft-lb/in | Average value: 6.53 J/cm Grade Count:10 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is .. |
|||
Izod Impact, Unnotched | 6.41 - 8.54 J/cm | 12.0 - 16.0 ft-lb/in | Average value: 7.35 J/cm Grade Count:4 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |
|||
Izod Impact, Unnotched | 2.67 - 8.54 J/cm | 5.00 - 16.0 ft-lb/in | Average value: 5.49 J/cm Grade Count:21 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi.. |
|||
Izod Impact, Unnotched | 0.747 - 8.54 J/cm | 1.40 - 16.0 ft-lb/in | Average value: 4.35 J/cm Grade Count:79 |
Overview of materials for Polypropylene with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i.. |
|||
Izod Impact, Unnotched | 1.60 - 8.54 J/cm | 3.00 - 16.0 ft-lb/in | Average value: 5.23 J/cm Grade Count:73 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |