Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.14 - 7.47 J/cm | 4.00 - 14.0 ft-lb/in | Average value: 3.36 J/cm Grade Count:17 |
Overview of materials for Polyphthalamide (PPA), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Aramid Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Izod Impact, Unnotched | 0.374 - 7.47 J/cm | 0.700 - 14.0 ft-lb/in | Average value: 3.28 J/cm Grade Count:13 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
Izod Impact, Unnotched | 4.27 - 7.47 J/cm | 8.00 - 14.0 ft-lb/in | Average value: 5.87 J/cm Grade Count:4 |
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an.. |
|||
Izod Impact, Unnotched | 2.67 - 7.47 J/cm | 5.00 - 14.0 ft-lb/in | Average value: 4.98 J/cm Grade Count:34 |
Overview of materials for Acetal Copolymer + Glass/PTFE This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer + Glass/PTFE". Each property range of values reported is minimum and maximum values of .. |
|||
Izod Impact, Unnotched | 1.87 - 7.47 J/cm | 3.50 - 14.0 ft-lb/in | Average value: 5.99 J/cm Grade Count:16 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Izod Impact, Unnotched | 3.74 - 7.47 J/cm | 7.00 - 14.0 ft-lb/in | Average value: 5.91 J/cm Grade Count:13 |
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% .. |
|||
Izod Impact, Unnotched | 3.47 - 7.47 J/cm | 6.50 - 14.0 ft-lb/in | Average value: 5.62 J/cm Grade Count:6 |
Overview of materials for Polyphthalamide (PPA), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Izod Impact, Unnotched | 1.60 - 7.47 J/cm | 3.00 - 14.0 ft-lb/in | Average value: 3.76 J/cm Grade Count:34 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |