Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.1356 - 2.1356 J/cm @Temperature -40.0 - -40.0 °C |
4.0009 - 4.0009 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 2.14 J/cm Grade Count:1 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Unnotched | 0.58729 - 2.1356 J/cm @Temperature -40.0 - -40.0 °C |
1.1002 - 4.0009 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 1.14 J/cm Grade Count:8 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Sheet". Each property range of values reported is minimum and max.. |
|||
Izod Impact, Unnotched | 2.1356 - 2.1356 J/cm @Temperature -18.0 - -18.0 °C |
4.0009 - 4.0009 ft-lb/in @Temperature -0.400 - -0.400 °F |
Average value: 2.14 J/cm Grade Count:1 |
Overview of materials for Polypropylene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Izod Impact, Unnotched | 2.02882 - 2.1356 J/cm @Temperature -18.0 - -18.0 °C |
3.80081 - 4.0009 ft-lb/in @Temperature -0.400 - -0.400 °F |
Average value: 2.06 J/cm Grade Count:3 |
Overview of materials for Polypropylene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of.. |