Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 6.41 - 10.1 J/cm | 12.0 - 19.0 ft-lb/in | Average value: 7.53 J/cm Grade Count:10 |
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35.. |
|||
Izod Impact, Unnotched | 7.47 - 10.1 J/cm | 14.0 - 19.0 ft-lb/in | Average value: 8.68 J/cm Grade Count:4 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Izod Impact, Unnotched | 9.10 - 10.1 J/cm | 17.0 - 19.0 ft-lb/in | Average value: 9.74 J/cm Grade Count:4 |
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled". Each property range of values reported i.. |
|||
Izod Impact, Unnotched | 1.57 - 10.1 J/cm | 2.94 - 19.0 ft-lb/in | Average value: 7.43 J/cm Grade Count:29 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Izod Impact, Unnotched | 4.27 - 10.1 J/cm | 8.00 - 19.0 ft-lb/in | Average value: 6.89 J/cm Grade Count:10 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
Izod Impact, Unnotched | 7.47 - 10.1 J/cm | 14.0 - 19.0 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 1200H-24 Polyester SMC
(discontinued **) Premi-Glas® 1200H-24 is a 24% fiberglass reinforced, thermoset, Sheet Molding Compound designed for applications where arc resistance and dielectric strength are required and UL 94 HB flame recogni.. |