Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 8.11 J/cm @Temperature 23.0 °C |
15.2 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Lubricomp DFP22 PC LNP* DFP22 is a Polycarbonate base resin containing glass fiber and PTFE/Silicone Lubricants. Characteristic of this grade is: Internally Lubricated.This data was supplied by SABIC-IP for the Amer.. |
|||
Izod Impact, Unnotched | 8.11 J/cm | 15.2 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP LF008 PEEK LNP* THERMOCOMP* LF008 is a compound based on Polyetheretherketone resin containing 40% Glass Fiber. |
|||
Izod Impact, Unnotched | 8.11 J/cm | 15.2 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP LF008 PEEK (Asia Pacific) LNP* Thermocomp* LF008 is a compound based on Polyetheretherketone resin containing Glass Fiber. |