Polymer Property : Izod Impact, Unnotched = 5.19 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 5.19 J/cm
9.72 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP EC005R PEI
LNP* THERMOCOMP* EC005R is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features include: Mold Release, Electrically Conductive.