Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 5.03 J/cm | 9.42 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP KFL32L Acetal Copolymer LNP* LUBRICOMP* KFL32L is a compound based on Acetal Copolymer resin containing 10% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Unnotched | 5.03 J/cm @Temperature 23.0 °C |
9.42 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Lubricomp KFL32L Acetal Copolymer (Asia Pacific) LNP* Lubricomp* KFL32L is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible.This data was supp.. |