Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.64 - 5340 J/cm | 8.69 - 10000 ft-lb/in | Average value: 8.60 J/cm Grade Count:47 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |
|||
Izod Impact, Unnotched | 4.64 J/cm | 8.69 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DE0069F PC LNP* STAT-KON* DE0069F is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Superior Molding. |
|||
Izod Impact, Unnotched | 4.64 J/cm @Temperature 23.0 °C |
8.69 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp WC006 Polyester, TP LNP* Thermocomp* WC006 is a compound based on Polyester, TP resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 4.64 J/cm | 8.69 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP WC006 Polyester, TP (Asia Pacific) LNP* Thermocomp* WC006 is a compound based on Polyester, TP resin containing Carbon Fiber. |
|||
Izod Impact, Unnotched | 4.64 J/cm | 8.69 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP WC006 PBT LNP* THERMOCOMP* WC006 is a compound based on PBT resin containing 30% Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
Izod Impact, Unnotched | 4.64 J/cm | 8.69 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Comtuf® 635 Nylon 6/6, Glass/Mineral Reinforced, Impact Modified, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has .. |
|||
Izod Impact, Unnotched | 4.64 J/cm | 8.69 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP DBL349E PC (Asia Pacific) LNP* Lubricomp* DBL349E is a compound based on Polycarbonate resin containing Glass Bead, PTFE, Flame Retardant. Added features of this material include:LNP* Lubricomp* DBL349E is a compound based .. |
|||
Izod Impact, Unnotched | 4.64 J/cm | 8.69 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP DBL349E PC LNP* Lubricomp* DBL349E is a compound based on Polycarbonate resin containing 20% Glass Bead, 15% PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retard.. |