Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 20.93 J/cm | 39.21 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DD0009P PC LNP STAT-KON* DD0009P is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Exceptional Processing, Flame Retardant... |
|||
Izod Impact, Unnotched | 20.93 J/cm | 39.21 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DD0009P PC (Asia Pacific) LNP STAT-KON* DD0009P is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched | 20.93 J/cm | 39.21 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DD0009PC PC (Europe-Africa-Middle East) LNP STAT-KON* DD0009PC is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |