Mechanical Properties Metric English Comments
Izod Impact, Unnotched 12.0 J/cm
22.5 ft-lb/in
ASTM D4812
Premix Premi-Glas® 2200-30 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2200-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Izod Impact, Unnotched 12.0 J/cm
22.5 ft-lb/in
ASTM D4812
Premix Premi-Glas® 2203-30 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2203-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Izod Impact, Unnotched 12.0 J/cm
22.5 ft-lb/in
ASTM D4812
Premix Premi-Glas® 2204-30 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2204-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Izod Impact, Unnotched 12.0 J/cm
22.5 ft-lb/in
ASTM D4812
Premix Premi-Glas® 2205-30 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2205-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Izod Impact, Unnotched 12.0 J/cm
22.5 ft-lb/in
ASTM D4812
Premix Premi-Glas® 3200-30 Fiberglass Reinforced SMC
Description: Premi-Glas® 3200-30 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di..
Izod Impact, Unnotched 12.0 J/cm
22.5 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Lexan® 505RU PC
Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro..
Izod Impact, Unnotched 12.0 J/cm
22.5 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Lexan® 505RU PC (Asia Pacific)
Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro..
Izod Impact, Unnotched 12.0 J/cm
22.5 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Lexan® 505RU PC (Europe-Africa-Middle East)
Lexan* 505RU is a 10% glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEE..