Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 1.72 J/cm @Temperature 23.0 °C |
3.22 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp WB006 PBT LNP* Thermocomp* WB006 is a compound based on Polybutylene Terephalate resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 1.72 - 6.41 J/cm | 3.22 - 12.0 ft-lb/in | Average value: 3.71 J/cm Grade Count:20 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |