Polymer Property : Izod Impact, Unnotched = 0.580 J/cm
Polymer Property :
Izod Impact, Unnotched =
0.580 J/cm
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Izod Impact, Unnotched
0.580
J/cm
1.09
ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Asia Pacific)
Thermally conductive mineral filled PPS FR compound