Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Creep Strength | 16.0 MPa @Time 360000 sec |
2320 psi @Time 100 hour |
in water at 95°C |
BASF Ultrason E 3010 PES Ultrason E 3010 is an unfilled, higher viscosity injection molding and extrusion PES grade, tougher and with improved chemical resistance. |