Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1650 MPa @Temperature 23.0 °C |
240000 psi @Temperature 73.4 °F |
D790B |
Ineos L06Z-00 Polypropylene Impact Copolymer This is a medium MFR impact copolymer polypropylene made for injection molded caps and closures applications. It offers a good balance of stiffness to impact resistance as compared to other impact .. |