Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Creep Strength | 10.0 MPa @Temperature 20.0 °C, Time 605000 sec |
1450 psi @Temperature 68.0 °F, Time 168 hour |
|
Okulen® 1000 - REG PE Colored OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Creep Strength | 10.0 MPa @Temperature 20.0 °C, Time 605000 sec |
1450 psi @Temperature 68.0 °F, Time 168 hour |
|
Okulen® 1000 - REG PE Multicoloured coarse OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Creep Strength | 10.0 MPa @Temperature 20.0 °C, Time 605000 sec |
1450 psi @Temperature 68.0 °F, Time 168 hour |
|
Okulen® 1000 PE-UHMW, AST OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Creep Strength | 10.0 MPa @Temperature 20.0 °C, Time 605000 sec |
1450 psi @Temperature 68.0 °F, Time 168 hour |
|
Okulen® 1000 PE-UHMW, Black OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Creep Strength | 10.0 MPa @Temperature 20.0 °C, Time 605000 sec |
1450 psi @Temperature 68.0 °F, Time 168 hour |
|
Okulen® 1000 PE-UHMW, Colored OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Creep Strength | 10.0 MPa | 1450 psi | |
Okulen® 1000 PE-UHMW, Conductive OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Creep Strength | 10.0 MPa | 1450 psi | |
Okulen® 1000 PE-UHMW, Green Black OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Creep Strength | 10.0 MPa | 1450 psi | |
Okulen® 1000 PE-UHMW, MoS2 -Moly- OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Creep Strength | 10.0 MPa | 1450 psi | |
Okulen® 1000 PE-UHMW, Multi-color OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Creep Strength | 10.0 MPa @Temperature 20.0 °C, Time 605000 sec |
1450 psi @Temperature 68.0 °F, Time 168 hour |
|
Okulen® 1000 PE-UHMW, Natural OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Creep Strength | 10.0 MPa @Temperature 20.0 °C, Time 605000 sec |
1450 psi @Temperature 68.0 °F, Time 168 hour |
|
Okulen® 1000 PE-UHMW, UV - stabilized OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Creep Strength | 10.0 MPa | 1450 psi | |
Okulen® 2000 PE-UHMW, 588 Blue OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Creep Strength | 10.0 MPa | 1450 psi | |
Okulen® 2000 PE-UHMW, AB OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Creep Strength | 10.0 MPa | 1450 psi | |
Okulen® 2000 PE-UHMW, DG OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Creep Strength | 10.0 MPa | 1450 psi | |
Okulen® 2000 PE-UHMW, DryRun OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Creep Strength | 10.0 MPa | 1450 psi | |
Okulen® 2000 PE-UHMW, L OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Creep Strength | 10.0 MPa | 1450 psi | |
Okulen® 2000 PE-UHMW, SL OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Creep Strength | 10.0 MPa @Temperature 20.0 °C, Time 605000 sec |
1450 psi @Temperature 68.0 °F, Time 168 hour |
|
Okulen® 500 - REG PE Multicoloured coarse OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Creep Strength | 10.0 MPa @Temperature 20.0 °C, Time 605000 sec |
1450 psi @Temperature 68.0 °F, Time 168 hour |
|
Okulen® 500 - REG PE Multicoloured fine OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Creep Strength | 10.0 MPa @Temperature 20.0 °C, Time 605000 sec |
1450 psi @Temperature 68.0 °F, Time 168 hour |
|
Okulen® 500 PE-HMW, AST OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Creep Strength | 10.0 MPa @Temperature 20.0 °C, Time 605000 sec |
1450 psi @Temperature 68.0 °F, Time 168 hour |
|
Okulen® 500 PE-HMW, Coloured OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Creep Strength | 10.0 MPa @Temperature 20.0 °C, Time 605000 sec |
1450 psi @Temperature 68.0 °F, Time 168 hour |
|
Okulen® 500 PE-HMW, UV - stabilized OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Creep Strength | 10.0 MPa @Temperature 20.0 °C, Time 605000 sec |
1450 psi @Temperature 68.0 °F, Time 168 hour |
|
Okulen® 1000 - REG PE Multicoloured fine OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Creep Strength | 10.0 MPa | 1450 psi | |
Okulen® 2000 PE-UHMW, OF OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Creep Strength | 10.0 MPa | 1450 psi | |
Okulen® 2000 PE-UHMW, W OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Creep Strength | >= 10.0 MPa | >= 1450 psi | 1% elongation, 1000 h; DIN 53444 |
Schwartz Technical Plastics LAMIGAMID® 307 Cast Polyamide 6, Heat Stabilized, Dry Application: slippers, inserts for coupling boxesInformation provided by Schwartz Technical Plastics GmbH |
|||
Creep Strength | >= 10.0 MPa | >= 1450 psi | 2% elongation, 1000 h; DIN 53444 |
Schwartz Technical Plastics LAMIGAMID® 320 Cast Polyamide 6, Conditioned Application: heavy-duty wheelsInformation provided by Schwartz Technical Plastics GmbH |
|||
Creep Strength | >= 10.0 MPa | >= 1450 psi | 2% elongation, 1000 h; DIN 53444 |
Schwartz Technical Plastics LAMIGAMID® 324 Cast Polyamide 6, MoS2, Heat Stabilized, Conditioned Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH |
|||
Creep Strength | >= 10.0 MPa | >= 1450 psi | 2% elongation, 1000 h; DIN 53444 |
Schwartz Technical Plastics LAMIGAMID® 327 Cast Polyamide 6, MoS2, Heat Stabilized, Conditioned Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH |
|||
Creep Strength | 10.0 MPa @Temperature 20.0 °C, Time 605000 sec |
1450 psi @Temperature 68.0 °F, Time 168 hour |
|
Okulen® 500 PE-HMW, Natural OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |