Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 77.0 MPa @Temperature 163 °C |
11200 psi @Temperature 325 °F |
Wet (7 day immersion at 71°C) |
Hexcel® HexPly® 954-3 Curing Cyanate Resin HexPly® 954-3 is a 350°F (177°C) curing cyanate resin with excellent resistance to moisture absorption, outgassing and microcracking. HexPly® 954-3 is formulated for autoclave or press molding u.. |