Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 201 MPa @Strain 3.50 % |
29200 psi @Strain 3.50 % |
ISO 178 |
Lanxess Durethan® BKV 15 H3.0 000000 Nylon 6 Copolymer, 15% Glass Fibers PA 6 Copolymer, 15% glass fibers, injection molding, heat-ageing stabilized |