Polymer Property : Charpy Impact Unnotched = 32.8 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 4.00 - 6.90 J/cm²

@Temperature -30.0 - 30.0 °C
19.0 - 32.8 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 5.95 J/cm² Grade Count:13
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45..