Polymer Property : Charpy Impact Unnotched = 1.43 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 0.300 - 0.400 J/cm²
1.43 - 1.90 ft-lb/in²
Compression; ISO 179/1eU
Raschig Group RALUPOL® 4566 UP Polyester
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u..
Charpy Impact Unnotched 0.300 J/cm² - NB
1.43 ft-lb/in² - NB
Average value: 7.79 J/cm² Grade Count:116
Overview of materials for Polypropylene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri..
Charpy Impact Unnotched 0.300 J/cm²

@Temperature 23.0 °C
1.43 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/2 eU
Hexion Bakelite™ PF 13 Phenolic Formaldehyde Resin, UL Listed  (discontinued **)
Phenolic molding compound, inorganically mica filled, heat resistance, good electrical properties, UL listed molding compound 0.75 mm/V-1 (NC), 3 mm/V-0, standardized molding compound.Application ar..
Charpy Impact Unnotched 0.300 J/cm²
1.43 ft-lb/in²
IS0179-1:2000
Zhejiang Juner PP8 PP For Automotive Parts
Applications: Air Conditioning SystemInformation provided by Zhejiang Juner New Materials Co, Ltd.
Charpy Impact Unnotched >= 0.300 J/cm²
>= 1.43 ft-lb/in²
Parallel to laminations; IEC 1212-2 5.5.2
Hippe MF CC 201 Woven Cotton Cloth Reinforced Melamine Resin - Sheet
Used in mechanical and electrical applications (coarse weave: >130 g/m2, =30 threads/cm). Arc and tracking resistant.Information provided by Hippe.
Charpy Impact Unnotched 0.300 J/cm² - NB

@Temperature -40.0 - -20.0 °C
1.43 ft-lb/in² - NB

@Temperature -40.0 - -4.00 °F
Average value: 6.53 J/cm² Grade Count:61
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma..
Charpy Impact Unnotched 0.300 J/cm²

@Temperature -30.0 °C
1.43 ft-lb/in²

@Temperature -22.0 °F
Ineos ABS NOVODUR® P2T ABS, Injection Grade  (discontinued **)
Injection molding grade, very high heat resistance.Applications: Automotive industry, household appliances.Information provided by the manufacturer.Novodur is produced by Styrolution (2014). This g..