Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 2.50 - 4.70 J/cm² | 11.9 - 22.4 ft-lb/in² | Average value: 3.85 J/cm² Grade Count:4 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Charpy Impact Unnotched | 1.00 - 4.70 J/cm² @Temperature -20.0 - -20.0 °C |
4.76 - 22.4 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 2.98 J/cm² Grade Count:4 |
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and.. |